⊙ Typical Properties |
|||
Test Items |
CASMOLY PL-30(G) |
Test Method |
|
Appearance |
White /Green |
- |
|
NLGI |
1 |
- |
|
Worked Penetration (25℃) |
310~340 |
ASTM D 217 |
|
Dropping Point (℃) |
205 |
ASTM D 566 |
|
Copper strip corrosion |
1a |
ASTM D 4048 |
|
Oil Separation (wt%) |
5.0 |
ASTM D 6184 |
|
Oxidation stability (kg/㎠) |
0.15 |
ASTM D 942 |
|
Polystyrene reaction test (60℃*24hour) |
No change |
- |
|
4 Ball E.P. (kg) |
315 |
ASTM D 2596 |
|
4 Ball wear (mm) |
0.45 |
ASTM D 2266 |
|
Low Temperature Torque test (-30℃,gf.cm) |
Starting |
290 |
ASTM D 1478 |
Running |
140 |