PA6日本宇部 1013NW8标准粘度高速结晶
规格级别
注塑
外观颜色
该料用途
备注说明
特性:标准粘度高速结晶
加工条件
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
基本性能 | 吸水率 | ASTM D-570 | 10.7 | % | |
成型收缩率 | UBEmethod | 1.3 | % | ||
吸水率 | ASTM D-570 | 1.8 | % | ||
成型收缩率 | UBEmethod | 1.2 | % | ||
物理性能 | 比重 | ASTM D-792 | 1.14 | ||
机械性能 | 硬度(洛氏、布氏) | 23° | ASTM D-785 | 120 | |
弯曲强度 | -30° | ASTM D-790 | 1400 | kgf/cm2 | |
挤剪强度 | 23° | ASTM D-732 | 650 | kgf/cm2 | |
1%变形下的压缩强度 | 23° | ASTM D-695 | 100 | kgf/cm2 | |
挤剪强度 | 23° | ASTM D-732 | 600 | kgf/cm2 | |
弯曲强度 | 23° | ASTM D-790 | 400 | kgf/cm2 | |
TABER磨耗率 | ASTM D-1044 | 7 | mg | ||
抗冲击强度 | 23° | ASTM D-256 | 50 | /cm | |
断裂下的伸张强度 | 23° | ASTM D-638 | 650 | kgf/cm2 | |
弯曲强度 | -30° | ASTM D-790 | 1300 | kgf/cm2 | |
弯曲强度 | 80° | ASTM D-790 | 260 | kgf/cm2 | |
屈服下的伸张强度 | -30° | ASTM D-638 | 1100 | kgf/cm2 | |
屈服下的延伸率 | 23° | ASTM D-638 | 8 | % | |
弯曲弹性率 | 80° | ASTM D-256 | 4000 | /cm | |
屈服下的伸张强度 | 23° | ASTM D-638 | 420 | kgf/cm2 | |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 85 | ||
1%变形下的压缩强度 | 23° | ASTM D-695 | 200 | kgf/cm2 | |
屈服下的伸张强度 | -30° | ASTM D-638 | 900 | kgf/cm2 | |
屈服下的伸张强度 | 80° | ASTM D-638 | 200 | kgf/cm2 | |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 55 | ||
抗冲击强度 | -30° | ASTM D-256 | 4.5 | /cm | |
断裂下的延伸率 | 23° | ASTM D-638 | 100 | % | |
屈服下的伸张强度 | 23° | ASTM D-638 | 800 | kgf/cm2 | |
断裂下的延伸率 | 23° | ASTM D-638 | >200 | % | |
弯曲弹性率 | -30° | ASTM D-790 | 29000 | kgf/cm2 | |
弯曲弹性率 | 23° | ASTM D-790 | 28500 | kgf/cm2 | |
弯曲强度 | 23° | ASTM D-790 | 1100 | kgf/cm2 | |
抗冲击强度 | 23° | ASTM D-256 | 6.5 | /cm | |
弯曲强度 | 80° | ASTM D-790 | 500 | kgf/cm2 | |
屈服下的伸张强度 | 80° | ASTM D-638 | 320 | kgf/cm2 | |
弯曲弹性率 | -30° | ASTM D-790 | 30000 | kgf/cm2 | |
弯曲弹性率 | 23° | ASTM D-790 | 7700 | kgf/cm2 | |
弯曲弹性率 | 80° | ASTM D-790 | 7500 | kgf/cm2 | |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 85 | ||
电气性能 | 介电常数 | 103HZ | ASTM D-150 | 8.0 | |
介电损耗 | 106HZ | ASTM D-150 | 0.02 | ||
体积电阻率 | ASTM D-257 | 1012 | Ω.cm | ||
介电常数 | 60HZ | ASTM D-150 | 9.0 | ||
IEC电路 | UL746 | 600+ | V | ||
介电常数 | 60HZ | ASTM D-150 | 3.9 | ||
介电常数 | 106HZ | ASTM D-150 | 3.5 | ||
介电损耗 | 103HZ | ASTM D-150 | 0.10 | ||
抗电弧强度 | ASTM D-495 | 119 | S | ||
介电常数 | 103HZ | ASTM D-150 | 3.8 | ||
介电损耗 | 103HZ | ASTM D-150 | 0.02 | ||
绝缘耐力 | ASTM D-149 | 20 | KV/mm | ||
介电损耗 | 60HZ | ASTM D-150 | 0.10 | ||
介电损耗 | 106HZ | ASTM D-150 | 0.12 | ||
介电常数 | 106HZ | ASTM D-150 | 4.5 | ||
介电损耗 | 60HZ | ASTM D-150 | 0.01 | ||
体积电阻率 | ASTM D-257 | 1015 | Ω.cm | ||
热性能 | 热变形温度 | 18.6kgf/cm2 | ASTM D-648 | 75 | °C |
熔点 | DSC | 215-225 | °C | ||
线性热膨胀系数 | ASTM D-696 | 8 | X的10-5cm/cm/°C | ||
热变形温度 | 4.6kgf/cm2 | ASTM D-648 | 180 | °C | |
燃烧率 | UL94 | V-2 |