309LMo''型抗腐蚀焊丝。OK Tigrod 309MoL适用于非合金和低合金钢的堆焊,以及诸如将316L焊接到非合金钢和低合金钢等以钼作为重要元素的异种钢焊接。
Typical Tensile Properties
As welded | ||
Elongation | Tensile Strength | Yield Strength |
26 % | 630 MPa | 510 MPa |
夏比V型缺口冲击性能
As welded | |
Impact Value | Testing Temperature |
90 J | 20 °C |
焊缝金属分析
Mn | ||||||
Mn | Mo | Cu | C | Si | Ni | Cr |
1.5 % | - | - | - | - | - | - |
Mo | ||||||
Mn | Mo | Cu | C | Si | Ni | Cr |
- | 2.5 % | - | - | - | - | - |
Cu | ||||||
Mn | Mo | Cu | C | Si | Ni | Cr |
- | - | 0.12 % | - | - | - | - |
C | ||||||
Mn | Mo | Cu | C | Si | Ni | Cr |
- | - | - | 0.01 % | - | - | - |
Si | ||||||
Mn | Mo | Cu | C | Si | Ni | Cr |
- | - | - | - | 0.4 % | - | - |
Ni | ||||||
Mn | Mo | Cu | C | Si | Ni | Cr |
- | - | - | - | - | 14.6 % | - |
Cr | ||||||
Mn | Mo | Cu | C | Si | Ni | Cr |
- | - | - | - | - | - | 21.4 % |